참여 물질
| 역할 | 이름 | HCID | 투입량 |
|---|
| 반응물 | Urethane acrylate | HCID 21863578 | — |
| 반응물 | Dipentaerythritol caprolactone | HCID 66608674 | — |
| 반응물 | Pentaerythritol hexaacrylate | HCID 131731916 | — |
| 용매 | Isopropanol | HCID 3776 | — |
| 생성물 | 1-Hydroxycyclohexyl phenyl ketone | HCID 70355 | — |
반응 단계
A protective layer coating solution was prepared by mixing 3 parts by mass of pentaerythritol hexaacrylate (KAYARAD DPHA, produced by Nippon Kayaku Co., Ltd.), 3 parts by mass of an urethane acrylate oligomer (ART RESIN UN-3320HA, produced by Negami Chemical Industrial Co., Ltd.), 3 parts by mass of an acrylic acid ester of dipentaerythritol caprolactone (KAYARAD DPCA-120, produced by Nippon Kayaku Co., Ltd.), 1 part by mass of a silica (P-526, produced by Mizusawa Industrial Chemicals, Ltd.), 0.5 parts by mass of a photopolymerization initiator (IRGACURE 184, produced by Nihon Ciba-Geigy K.K.), and 11 parts by mass of isopropyl alcohol, and sufficiently agitating and dispersing the mixture with the use of a ball mill, such that the average particle diameter became approximately 3 μm.
출처 및 근거
| DOI | 10.6084/m9.figshare.5104873.v1 |
|---|
| 특허 번호 | US08852856B2 |
|---|
| 출처 데이터셋 | uspto-grants-2014_10 |
|---|
| ORD ID | ord-8b9d069eb1fd492a9b508b48fd643f04 |
|---|