Ethylene → Ethylene

HRID 596714
인쇄

반응식

HRID 596714 반응식
[CH:1]([Al])=[CH:2]C(=C)C.C=C.[CH3:9][CH2:10][CH2:11][CH3:12].[CH3:13][CH2:14][CH:15]=[CH2:16].[H][H]>[Cl-].[Cl-].[Cl-].[Ti+3]>[CH2:1]=[CH2:2].[CH3:12][CH2:11][CH:10]=[CH2:9].[CH3:13]/[CH:14]=[CH:15]/[CH3:16]
참가 물질실험 절차출처 및 근거반응 노트

참가 물질

10

반응물 6

HCID 6325Ethylene2회HCID 7843ButaneHCID 78441-ButeneHCID 57352863CID 57352863HCID 178418361HCID 178418361, 화합물HCID 178435160HCID 178435160, 화합물

생성물 3

HCID 6325Ethylene
HCID 7844
1-Butene
HCID 62695trans-2-BUTENE

시약·촉매·용매 1

HCID 10313229titanium(III) trichloride촉매

실험 절차

With the aid of a mixed catalyst of 0.0015 part by weight of this titanium trichloride catalyst and 0.016 part by weight of isoprenylaluminum, 11.5 parts by weight of ethene is first polymerized for 1/2 hour under a pressure of 7-8 atmospheres gauge in 15 parts by weight of a C4 -cut containing 38.4% trans-butene-2, 28.8% cis-butene-2, 32.5% butane and 0.3% butene-1 at a temperature of 50° C. Thereafter, 0.002 part by weight of hydrogen is added thereto. Under a total pressure of 8-10 atm. gauge, the polymerization is continued. The ethene is added during the entire polymerization time of 21/2 hours. Subsequently, the polyethylene suspension is expanded via nozzles into a second container, thus obtaining 11.1 parts by weight of a terpolymer of ethene, butene-1 and butene-2 with the following properties:

출처 및 근거

ORD 기록
ord-d7db48530ade4b0f9570fd0f4ad49a30
출처 데이터셋
uspto-grants-1977_03
DOI
10.6084/m9.figshare.5104873.v1
특허 번호
US04011384