| 역할 | 이름 | HCID | 투입량 |
|---|
| 반응물 | Aluminum Stearate | HCID 12496 | — |
| 반응물 | Aluminum | HCID 5359268 | — |
| 반응물 | Sodium | HCID 5360545 | — |
| 반응물 | Sodium brassylate | HCID 11514768 | — |
| 생성물 | Ethylene brassylate | HCID 61014 | 88.1% |
반응 단계
Sodium brassylate (0.33 gram) and aluminum stearate (1.09 gram) were added to 70 grams poly(ethylene brassylate) and the mixture heated at 200° C. until a homogeneous viscous mass was obtained. The molar ratio of sodium to aluminum was 2:1. The temperature was then increased to 312° C. and the pressure reduced to 0.3-0.5 mm Hg. The depolymerization reaction was complete in about 3 hours and 88.1 percent yield ethylene brassylate was obtained.