Ammonium Oxalate → Cerous oxalate

https://huagongshe.com/ko/reaction/6307

반응식

참여 물질

역할이름HCID투입량
반응물Ammonium OxalateHCID 14213—
반응물Cerium nitrateHCID 24948—
촉매Cobalt(II) chlorideHCID 24288—
생성물Cerous oxalateHCID 165565—

반응 조건

온도35 °C

반응 단계

A solution of cobalt chloride having a gravity of 1.05 g/cm3 was mixed with a solution of cerium nitrate and heated to 35° C., followed by adding, while stirring a solution of ammonium oxalate having a gravity of 1.03 g/m3 and a pH 3. The quantity of ammonium oxalate added was 1.5 mole equivalent per mole equivalent of cobalt chloride and cerium nitrate. The precipitates of cobalt oxalate and cerium oxalate were obtained after reaction and filtrated in a vacuum filtrator to remove the mother liquid, washed by distilled water of 90° C. for 6 times, dried at 200° C., crushed and sieved by a 20 mesh sieve, reduced at 550° C. in hydrogen for 3 h, then crushed again and sieved by a 100 mesh sieve. The prepared cobalt powder contained 0.5% (wt.) cerium.

출처 및 근거

DOI10.6084/m9.figshare.5104873.v1
특허 번호US05248328
출처 데이터셋uspto-grants-1993_09
ORD IDord-ba07d0f4cc294f878e1a0259559fe581
출처 메모uspto-grants-1993_09