Ammonium Oxalate → Samarium oxalate

https://huagongshe.com/ko/reaction/6309

반응식

참여 물질

역할이름HCID투입량
반응물Ammonium OxalateHCID 14213—
반응물Samarium nitrateHCID 25205—
촉매Cobalt(II) chlorideHCID 24288—
생성물Samarium oxalateHCID 165093—

반응 조건

온도70 °C

반응 단계

A solution of cobalt chloride having a gravity of 1.10 g/cm3 was mixed homogeneously with a solution of samarium nitrate having a concentration of 94 mg/ml in a volume proportion of 150:1. The mixed solution was heated to 70° C. A solution of ammonium oxalate having a gravity of 1.15 g/cm3 and a pH value of 5 was added to the mixture while stirring. The quantity of the added ammonium oxalate was 1.7 mole equivalent per mole equivalent cobalt chloride and samarium nitrate. The precipitates of cobalt oxalate and samarium oxalate were obtained after reaction, then filtrated in a vacuum filtrator to remove the mother liquid, washed by distilled water of 90° C. for 6 times, dried at 200° C., crushed and sieved by a 20 mesh sieve, reduced at 530° C. in hydrogen for 4 h, crushed again and sieved by a 100 mesh sieve.

출처 및 근거

DOI10.6084/m9.figshare.5104873.v1
특허 번호US05248328
출처 데이터셋uspto-grants-1993_09
ORD IDord-042063d63f8a444cbb89063f7771e99d
출처 메모uspto-grants-1993_09