참여 물질
| 역할 | 이름 | HCID | 투입량 |
|---|
| 반응물 | Ethyl Methacrylate | HCID 7343 | — |
| 반응물 | Propylene glycol methyl ether acetate | HCID 7946 | — |
| 반응물 | 3-Hydroxypropyl methacrylate | HCID 17694 | — |
| 반응물 | Methylanthracene methacrylate | HCID 87125978 | — |
| 생성물 | 2-Hydroxypropyl methacrylate | HCID 13539 | — |
반응 단계
A polymer feed solution was prepared by combining 30.76 g methylanthracene methacrylate monomer, 16.6 g 3-hydroxypropyl methacrylate monomer, 16.0 g ethyl methacrylate, and 50 g propylene glycol monomethyl ether acetate (PGMEA) in a 250 ml three neck, round-bottom flask fitted with a mechanical stirrer, thermal controller, thermal probe, heating mantle and nitrogen purge inlet (sweep). The reaction mixture was heated until the temperature of the reaction mixture reached 80° C. 16.15 g PGMEA solution containing 10 wt % Vazo 67 azo initiator (white powder, Dupont) was next added to the flask. The flask was heated until the temperature of the reaction mixture reached 90° C. and maintained for 8 hours with stirring. Heating was stopped and the reactor was allowed to cool down to 40° C. The resulting polymer solution was precipitated with methyl alcohol (10× excess of reaction mixture), filtered and vacuum dried, to provide Poly(ANTMA-co-HPMA-co-EMA) polymer [Mw=8K; PDI=2.5; ANTMA:HPMA; EMA=30:30:40 mol %, by 13C-NMR].
출처 및 근거
| DOI | 10.6084/m9.figshare.5104873.v1 |
|---|
| 특허 번호 | US09324604B2 |
|---|
| 출처 데이터셋 | uspto-grants-2016_04 |
|---|
| ORD ID | ord-c9da4760507f4314a70b74da3feaa588 |
|---|
| 출처 메모 | uspto-grants-2016_04 |
|---|