반응식
[C:1]1([CH3:9])[C:2]([NH2:8])=[CH:3][C:4]([NH2:7])=[CH:5][CH:6]=1.C1C2C3C=CC(C2C=C1)C3.[CH3:20][CH2:21][CH2:22][CH2:23][CH3:24]>>[CH:22]1([C:5]2[CH:6]=[C:1]([CH3:9])[C:2]([NH2:8])=[CH:3][C:4]=2[NH2:7])[CH2:23][CH2:24][CH:20]=[CH:21]1참가 물질
4
반응 조건
- 온도
- 205 °C
실험 절차
A 200 g (1.64 mol) portion of 2,4-toluenediamine, 162 g (1.23 mol, 2.45 equiv) of dicyclopentadiene, 200 g (2.78 mol) of pentane, and 20.0 g of an amorphous alumina-silica catalyst comprised of 13% alumina and 87% silica were charged to a 1000 cc pressure vessel equipped with a mechanical stirrer. The vessel was sealed and purged with nitrogen leaving a 32 psig nitrogen blanket. The vessel contents were heated to 205° C. with stirring and were maintained at that temperature for 22 hr. The contents were cooled to 150° C. and isoIated catalyst free by hot filtration. Selective removal of residual hydrocarbons by vacuum distillation and analysis by gas chromatography (GC) revealed the following product mixture:
후처리
- additionwere charged to a 1000 cc pressure vessel
- customequipped with a mechanical stirrer
- customThe vessel was sealed
- custompurged with nitrogen leaving a 32 psig nitrogen blanket
- temperaturewere maintained at that temperature for 22 hr
- temperatureThe contents were cooled to 150° C.
- filtrationisoIated catalyst free by hot filtration
- customremoval of residual hydrocarbons
- distillationby vacuum distillation and analysis by gas chromatography (GC)
출처 및 근거
- ORD 기록
- ord-4d18f717f53244abb626cda2249ca69b
- 출처 데이터셋
- uspto-grants-1991_01
- 특허 번호
- US04985159