돌아가기
Huagongshe화공사 화학 정보 인쇄 보고서 · 연구 참고용
HRID 83936생성일: 2026년 10월 25일

Acrylic Acid → alpha-Methylene-gamma-butyrolactone acrylic acid pentaerythritol allyl ether

https://huagongshe.com/reaction/83936

반응식

참여 물질

역할이름HCID투입량
반응물Acrylic AcidHCID 6581—
반응물Sodium HydroxideHCID 14798—
반응물Sodium PersulfateHCID 62655—
반응물alpha-Methylene butyrolactoneHCID 68352—
반응물Allyl pentaerythritolHCID 3086330—
반응물Sodium Lauryl SulfateHCID 3423265—
용매WaterHCID 962—
생성물alpha-Methylene-gamma-butyrolactone acrylic acid pentaerythritol allyl etherHCID 131731900—

반응 조건

온도75 °C

반응 단계

The crosslinked polymer poly(α-methylene-γ-butyrolactone-acrylic acid-pentaerythritol allyl ether) was prepared by emulsion polymerization of α-methylene-γ-butyrolactone and acrylic acid with the crosslinking monomer pentaerythritol allyl ether. To a four neck round bottom glass flask, equipped with a mechanical stirrer and a thermocouple with a nitrogen inlet at the side of the inlet-tube and two dropping funnels was added the initial charge of 44.03 g of water and 0.51 g of a 20% solution of sodium dodecyl sulfate surfactant. Into the monomer dropping funnel a mixture of 20.8 g of α-methylene-γ-butyrolactone, 1.1 g of acrylic acid and 0.16 g of pentaerythritol allyl ether were added. Into the second dropping funnel the aqueous mixture consisting of 83.43 g water, 1.32 g 20% sodium dodecylsulfate, 0.14 g sodium persulfate and 0.17 g 20% sodium hydroxide solution were added. The initial charge was heated to 75° C. dropwise addition of the monomer was started. Dropwise addition of the aqueous mixture started 5 minutes later. The monomer feed ended 120 minutes after the start of monomer addition, and the aqueous stream ended 5 minutes after the monomer stream ended. After a cook-down time of one hour, the reaction mixture was cooled to room temperature.

출처 및 근거

DOI10.6084/m9.figshare.5104873.v1
특허 번호US08846817B2
출처 데이터셋uspto-grants-2014_09
ORD IDord-40aa735a4fc642b2855ba315df9fa102
출처 메모uspto-grants-2014_09