참여 물질
| 역할 | 이름 | HCID | 투입량 |
|---|
| 반응물 | Water | HCID 962 | — |
| 반응물 | Acrylonitrile | HCID 7855 | — |
| 반응물 | Di-tert-butyl peroxide | HCID 8033 | — |
| 반응물 | alpha-Methylene butyrolactone | HCID 68352 | — |
| 반응물 | Sodium 4-styrenesulfonate | HCID 3571582 | — |
| 생성물 | alpha-Methylene-gamma-butyrolactone acrylonitrile p-styrene sulfonate | HCID 86762801 | — |
반응 단계
To a high-pressure stainless steel reactor with overhead stirring is added 7.82 g (0.147 mol) of acrylonitrile, 7.82 g (7.97×10−2 mol) of α-methylene-γ-butyrolactone, 0.50 g (2.42×10−3 mol) of sodium p-styrene sulfonate and 36.88 g (2.05 mol) of water. The reactor is purged with nitrogen and 0.78 g (5.33×10−3 mol) di-tert-butyl peroxide is added to the reaction mixture before the reactor is tightly closed and heated to 160° C. After 10 minutes at 160° C., the polymerization is allowed to cool to room temperature before drying the polymer under vacuum at elevated temperature for isolation.
출처 및 근거
| DOI | 10.6084/m9.figshare.5104873.v1 |
|---|
| 특허 번호 | US08846817B2 |
|---|
| 출처 데이터셋 | uspto-grants-2014_09 |
|---|
| ORD ID | ord-3ce3c6904c8c4ded9cf8fea90d96f1ec |
|---|
| 출처 메모 | uspto-grants-2014_09 |
|---|