홈MCP워크벤치Skills
홈워크벤치알림마이페이지
llms.txt · MCP 가이드개인정보처리방침 · 이용약관 · 지원v1.8.3
  1. 홈
  2. /반응

Lactic Acid → Lactic acid itaconic acid

HRID 853959
인쇄

반응식

HRID 853959 반응식
[C:1]([OH:6])(=[O:5])[C@H:2]([CH3:4])[OH:3].[C:7]([OH:15])(=[O:14])[C:8]([CH2:10][C:11]([OH:13])=[O:12])=[CH2:9].OCC(CO)(CO)CO.[Sn+2].C(O)(=O)C(C)O>>[C:1]([OH:6])(=[O:5])[CH:2]([CH3:4])[OH:3].[C:7]([OH:15])(=[O:14])[C:8]([CH2:10][C:11]([OH:13])=[O:12])=[CH2:9]
참가 물질반응 조건실험 절차후처리출처 및 근거반응 노트

참가 물질

6

반응물 5

HCID 612Lactic AcidHCID 811Itaconic acidHCID 8285PentaerythritolHCID 104883Stannous cationHCID 107689L-Lactic Acid

생성물 1

HCID 86597549Lactic acid itaconic acid

반응 조건

온도
180 °C

실험 절차

Into a 2 litre Rotavapor equipment used as the reactor was added 437.5 g L-lactic acid (88% water solution corresponding to 89 mole-%), 47.9 g itaconic acid (9 mol-%), 14.5 g pentaerythritol (2 mole-%) and 0.19 g tin(II) octoate. Dry nitrogen was led into the reactor and 500 mbar absolute pressure was established. The reactor vessel was partly immersed in an oil bath with a temperature of 90° C. The temperature of the oil bath was increased at a rate of 30° C./h to 120° C., and the reaction mixture was mixed by starting the rotation at a speed of 100 rpm. The temperature of the oil bath was evenly increased by 15° C./h until 180° C., where it was kept until the end of the polymerisation. The pressure was decreased every hour by the following steps: 500 (start)-500-450-400-350-290-190-140-90-60-50-40-30 mbar, at which pressure it was kept to the end of the polymerisation. Bubbling of nitrogen was continued throughout the polymerisation and the formed water was collected as it evolved. Total polymerisation time was 24 hours. During the polymerisation no lactide was formed on the reactor walls, condenser or receiver, although it typically forms in a condensation polymerisation of lactic acid.

후처리

  1. customThe reactor vessel was partly immersed in an oil bath with a temperature of 90° C
  2. temperatureThe temperature of the oil bath was increased at a rate of 30° C./h to 120° C.
  3. additionthe reaction mixture was mixed
  4. customwhere it was kept until the end of the polymerisation
  5. waitThe pressure was decreased every hour by the following steps
  6. custom500 (start)-500-450-400-350-290-190-140-90-60-50-40-30 mbar, at which pressure it was kept to the end of the polymerisation
  7. customBubbling of nitrogen
  8. customwas continued throughout the polymerisation
  9. customthe formed water was collected as it
  10. customTotal polymerisation time
  11. customwas formed on the reactor walls, condenser or receiver, although it

출처 및 근거

ORD 기록
ord-0277ee7bc7eb45f5b6ed8ac6f6b00e24
출처 데이터셋
uspto-grants-2007_08
DOI
10.6084/m9.figshare.5104873.v1
특허 번호
US07256250B2

반응 노트

이 페이지에서참가 물질반응 조건실험 절차후처리출처 및 근거반응 노트