Terephthalic Acid → Bis(2-hydroxyethyl) terephthalate

HRID 864275
인쇄

반응식

HRID 864275 반응식
[C:1]([OH:12])(=[O:11])[C:2]1[CH:10]=[CH:9][C:5]([C:6]([OH:8])=[O:7])=[CH:4][CH:3]=1>C(O)CO>[C:1]([O:12][CH2:2][CH2:1][OH:11])(=[O:11])[C:2]1[CH:10]=[CH:9][C:5]([C:6]([O:8][CH2:5][CH2:6][OH:7])=[O:7])=[CH:4][CH:3]=1
참가 물질실험 절차출처 및 근거반응 노트

참가 물질

3

반응물 1

HCID 7489Terephthalic Acid

생성물 1

HCID 13739Bis(2-hydroxyethyl) terephthalate

시약·촉매·용매 1

HCID 174Ethylene Glycol용매

실험 절차

Terephthalic acid was reacted with ethylene glycol to form bis-(2-hydroxyethyl) terephthalate and low oligomers thereof, in a standard direct esterification reaction. At the end of the direct esterification reaction 400 ppm of phosphoric acid stabiliser was added, followed by 500 ppm of antimony trioxide polycondensation catalyst and 500 ppm of "Irganox 1010" antioxidant. 0.3% of silica of particle size 4 μm, and 0.3% of titanium dioxide of particle size 0.2 μm were also added at this stage. A standard batch polycondensation reaction was performed until the intrinsic viscosity of the resultant polyethylene terephthalate was approximately 0.52. The polyethylene terephthalate was further polymerised by means of a batch solid phase polymerisation process, until the intrinsic viscosity (IV) of the polyethylene terephthalate was approximately 0.7 to 0.75. The solid phase polymerisation process utilised a fluidised bed, fluidised with nitrogen.

출처 및 근거

ORD 기록
ord-a2f9a7b3f9b94e5eb5167e5bd5f93d65
출처 데이터셋
uspto-grants-1996_10
DOI
10.6084/m9.figshare.5104873.v1
특허 번호
US05562984

반응 노트