돌아가기
Huagongshe화공사 화학 정보 인쇄 보고서 · 연구 참고용
HRID 896968생성일: 2026년 10월 27일

Methanol → HCID 178430148, 화합물

https://huagongshe.com/reaction/896968

반응식

참여 물질

역할이름HCID투입량
반응물MethanolHCID 887—
반응물WaterHCID 962—
반응물Potassium HydroxideHCID 14797—
반응물2-Methylprop-2-enoic acid;styreneHCID 165730—
반응물HCID 178430147HCID 178430147—
용매Dimethyl SulfoxideHCID 679—
용매PhthalimidineHCID 10199—
생성물HCID 178430148HCID 178430148—

반응 조건

온도0 °C

반응 단계

As a dispersing agent having a crosslinkable functional group, 9.5 parts of a styrene/methacrylic acid copolymer (acid value: 290; molecular weight: 15,000) were dissolved in 80 parts of dimethyl sulfoxide, and 10 parts of an isoindolinone pigment (C.I. Pigment Yellow 109) were suspended in the resultant solution in a flask at 25° C. under an air atmosphere. A 30% methanol solution of potassium hydroxide was then added dropwise little by little to dissolve the isoindolinone pigment. After the pigment solution was stirred for 3 hours, p-phenylene-bis(ethyl)carbodiimide as a crosslinking agent was added to and dissolved in the pigment solution in a proportion of 1 part per 10 parts of the pigment, and the resultant solution was quickly poured into ion-exchanged water (400 parts of ion-exchanged water per 10 parts of the pigment; 0° C.) stirred by an impellor type agitating blade (800 rpm), purged with nitrogen and cooled and temperature-maintained by means of 2 system dispensers (manufactured by Musashi Engineering K.K.; needle internal diameter: 0.57 mm; delivery pressure: 4.0 kgf/cm2) to obtain an aqueous dispersion of isoindolinone-pigment-containing particles having an average particle diameter of 35.6 nm. This aqueous dispersion was transferred to a reaction vessel equipped with a mantle heater, cooling tower, stirrer and thermometer, this system was purged with nitrogen with stirring at 300 rpm, 10% hydrochloric acid was added dropwise to adjust the pH of the reaction mixture to 4.75. After continuing the reaction for additional 5 hours, the resultant aggregates were filtered under reduced pressure through a membrane filter (holding particle diameter: 0.45 am) and washed 3 times with 500 ml of ion-exchanged water to obtain paste of an aqueous dispersion of the isoindolinone-pigment-containing particles desalted and desolvated.

출처 및 근거

DOI10.6084/m9.figshare.5104873.v1
특허 번호US06921433B2
출처 데이터셋uspto-grants-2005_07
ORD IDord-6a2ba8da322842529034ea6afa4759b0
출처 메모uspto-grants-2005_07