Huagongshe화공사 화학 정보 인쇄 보고서 · 연구 참고용
2,3-Dichloro-1,3-butadiene → Formaldehyde
참여 물질
| 역할 | 이름 | HCID | 투입량 |
|---|---|---|---|
| 반응물 | 2,3-Dichloro-1,3-butadiene | HCID 15447 | — |
| 반응물 | Resorcinol-formaldehyde resin | HCID 159980 | — |
| 반응물 | Sodium Lauryl Sulfate | HCID 3423265 | — |
| 용매 | Water | HCID 962 | — |
| 생성물 | Formaldehyde | HCID 712 | — |
| 생성물 | Resorcinol | HCID 5054 | — |
| 생성물 | Resorcinol-formaldehyde resin | HCID 159980 | — |
반응 단계
18.0 g of sodium lauryl sulfate (Emar 2F Needle (30% concentration), manufactured by Kao Corporation) was added as a surfactant to 295 g of the above 2,3-dichlorobutadiene homopolymer latex (2), and the mixture was thoroughly stirred until it became uniform. Then, 264.4 g of water was added thereto, and 656.4 g of the resorcinol/formaldehyde mixed liquid prepared as described above, was mixed thereto. The mixture was left to stand and aged at 23° C. for 24 hours to obtain a resorcinol/formaldehyde/latex mixed liquid (the weight ratio of the latex solid content to the sum of resorcinol and formaldehyde: 1/0.86, total amount of surfactant: 0.74 wt %).
출처 및 근거
| DOI | 10.6084/m9.figshare.5104873.v1 |
|---|---|
| 특허 번호 | US05766762 |
| 출처 데이터셋 | uspto-grants-1998_06 |
| ORD ID | ord-dfa1ef8ca5db49809baafea8708a917a |
| 출처 메모 | uspto-grants-1998_06 |