Ethylene → Ethene propene ethylidenenorbornene

HRID 991410

반응식

HRID 991410 반응식
[CH:1](=[C:3]1[CH2:8][C:7]2[CH2:9][CH:4]1[CH2:5][CH:6]=2)[CH3:2].[CH2:10]=[CH:11][CH3:12].C=C.B(C1C(F)=C(F)C(F)=C(F)C=1F)(C1C(F)=C(F)C(F)=C(F)C=1F)C1C(F)=C(F)C(F)=C(F)C=1F>C1(C)C=CC=CC=1>[CH2:1]=[CH2:2].[CH2:10]=[CH:11][CH3:12].[CH:1](=[C:3]1[CH2:8][CH:7]2[CH2:9][CH:4]1[CH:5]=[CH:6]2)[CH3:2]

참가 물질

6

반응 조건

온도
60 °C

실험 절차

A 2 L batch reactor is charged with 500 mL of mixed alkanes, 75 mL of 5-ethylidene-1-norbornene, and 500 mL of liquefied propylene. The reactor is heated to 60° C., and is saturated with ethylene at 500 psig (3.4 MPa). In an inert atmosphere drybox, 10 μmol of a 0.005M solution in toluene of rac-[1,2-ethanediylbis(1-(2-methyl-4-phenyl)indenyl)]zirconium (trans,trans-1,4-diphenyl-1,3-butadiene) and 10 μmol of a 0.005 m solution of B(C6F5)3 in toluene are combined and the mixture is transferred to the reactor to initiate polymerization. After 15 minutes, the reactor is vented and the solution is drained from the reactor. The polymer solution is combined with 100 mg of antioxidant and the volatiles are removed under reduced pressure in order to isolate the rubbery terpolymer of ethylene/propylene/ethylidene norbornene.

후처리

  1. custompolymerization
  2. customare removed under reduced pressure in order

출처 및 근거

ORD 기록
ord-4506bce7fcef45069ac5a372cb1c6f59
출처 데이터셋
uspto-grants-2002_10
특허 번호
US06465384B1

연결된 노트

불러오는 중…