Back
HuagongsheHuagongshe Chemistry Print Report · For research reference only
HRID 10115Generated: October 26, 2026

Ammonium Oxalate → Cerous oxalate

https://huagongshe.com/reaction/10115

Reaction equation

Participants

RoleNameHCIDCharge
ReactantAmmonium OxalateHCID 14213—
ReactantCerium(III) chlorideHCID 24636—
ReactantCerium oxideHCID 9905479—
ProductCerous oxalateHCID 165565—

Reaction Conditions

Temperature1500 °C

Reaction Steps

A cerium oxalate powder was prepared by adding an aqueous solution of ammonium oxalate to an aqueous solution of cerium chloride under stirring, causing the precipitation of cerium oxalate, filtering, and drying. The powder was ground with a jet-mill to obtain a starting material powder with a mean particle diameter of about 1 μm. The powder was ejected at a feed rate of 5 kg/hr through a nozzle with a cross-sectional area of the opening of 0.13 cm2 together with air at a flow rate of 200 L/min as a carrier gas into a reaction tube heated to a temperature of 1500° C. in an electric furnace, passed through the reaction tube, while maintaining the dispersion concentration of the powder, and heated. The melting point of cerium oxide is about 1950° C. The dispersion concentration of the starting material powder in the gas phase inside the reaction tube was 0.4 g/L, and V/S was 1500. The light-yellow powder thus produced was collected with a bag filter.

Provenance & Evidence

DOI10.6084/m9.figshare.5104873.v1
Patent numberUS07094289B2
Source datasetuspto-grants-2006_08
ORD IDord-c817a0ea0ac64877a846f4b006c3f5c4
Source noteuspto-grants-2006_08