HRID1016719

反应详情

EQUATION

反应方程式

HRID 1016719 的结构方程式

AUXILIARIES

试剂、催化剂与溶剂

1

CONDITIONS

反应条件

温度
85 °C

PROCEDURE

实验过程

Vanadium pentoxide (V2O5) (229 g) was added to water (500 mL), to thereby yield a mixture, and an aliquot of oxalic acid (477 g) was added to the mixture with stirring at 80-90° C. so as to dissolve the vanadium compound, to thereby yield a solution of vanadium oxalate. Another aliquot of oxalic acid (963 g) was added to water (400 mL), and the resultant mixture was heated to 50-60° C. To the mixture, a solution of chromic anhydride (CrO3) (252 g) in water (200 mL) was added under sufficient stirring so as to dissolve the components, to thereby yield a solution of chromium oxalate. The thus-yielded solutions were mixed at 50-60° C., to thereby prepare a V-Cr-containing solution. To the V-Cr-containing solution were added a solution of phosphomolybdic acid (H3(PMo12O40).20H2O) (41.1 g) dissolved in water (100 mL), and a solution of potassium acetate (CH3COOK) (4.0 g) dissolved in water (100 mL). Subsequently, a 20 wt. % aqueous silica sol (containing Na2O (0.02 wt. %)) (2,500 g) was added, to thereby form a slurry.

WORKUP

后处理

  1. customto thereby yield a mixture