Participants
| Role | Name | HCID | Charge |
|---|
| Reactant | Indene | HCID 7219 | — |
| Reactant | Alpha-Methylstyrene | HCID 7407 | — |
| Product | HCID 6713780 | HCID 6713780 | — |
Reaction Steps
A resin L-1 is prepared in a manner similar to that of preparing the resin I-1, except that 72 g of α-methylstyrene and 18 g of indene (that is, α-methylstyrene: 80 mass %, indene: 20 mass %) are used and that the addition of the catalyst is carried for 15 minutes and the polymerization reaction is allowed to proceed for 1 hour in a state where the temperature of the reaction mixed solution is maintained in the range of 6 to 8° C. The α-methylstyrene/indene copolymer resin thus obtained has yield: 79 g, softening point: 170° C., number-average molecular weight (Mn): 1000, and weight-average molecular weight (Mw): 3500.
Provenance & Evidence
| DOI | 10.6084/m9.figshare.5104873.v1 |
|---|
| Patent number | US08722806B2 |
|---|
| Source dataset | uspto-grants-2014_05 |
|---|
| ORD ID | ord-2c4ec02e581f4904a6341ce8db3f9acc |
|---|
| Source note | uspto-grants-2014_05 |
|---|