Back
HuagongsheHuagongshe Chemistry Print Report · For research reference only
HRID 1024132Generated: October 29, 2026

Alpha-Methylstyrene → HCID 86656477, compound

https://huagongshe.com/reaction/1024132

Reaction equation

Participants

RoleNameHCIDCharge
ReactantAlpha-MethylstyreneHCID 7407—
ReactantHCID 15354263HCID 15354263—
ProductHCID 86656477HCID 86656477—

Reaction Conditions

Temperature1.5 °C

Reaction Steps

A resin L-2a is prepared in a manner similar to that of preparing the resin B-2a, except that 72 g of α-methylstyrene and 8 g of 4-tert-butyl-α-methylstyrene (manufactured by Hokko Chemical Industry Co., Ltd.) are used in place of 80 g of 4, α-dimethylstyrene and that the dropwise dropwise addition of the catalyst is carried for 15 minutes and the polymerization reaction is allowed to proceed for 30 minutes in a state where the temperature of the reaction mixed solution is maintained in the range of 1 to 2° C. The resin L-2a thus obtained (α-methylstyrene/4-tert-butyl-α-methylstyrene copolymer) has yield: 50 g, softening point: 153° C., number-average molecular weight (Mn): 1350, and weight-average molecular weight (Mw): 3900.

Provenance & Evidence

DOI10.6084/m9.figshare.5104873.v1
Patent numberUS08722806B2
Source datasetuspto-grants-2014_05
ORD IDord-5cf43ecd95b14222bfd67653d41bbbf7
Source noteuspto-grants-2014_05