Back
HuagongsheHuagongshe Chemistry Print Report · For research reference only
HRID 1024133Generated: October 28, 2026

Alpha-Methylstyrene → HCID 86656477, compound

https://huagongshe.com/reaction/1024133

Reaction equation

Participants

RoleNameHCIDCharge
ReactantAlpha-MethylstyreneHCID 7407—
ReactantHCID 15354263HCID 15354263—
ProductHCID 86656477HCID 86656477—

Reaction Conditions

Temperature-3.5 °C

Reaction Steps

A resin M-2a is prepared in a manner similar to that of preparing the resin B-2a, except that 72 g of α-methylstyrene and 8 g of 4-tert-butyl-α-methylstyrene are used in place of 80 g of 4, α-dimethylstyrene and that the dropwise dropwise addition of the catalyst is carried for 15 minutes and the polymerization reaction is allowed to proceed for 30 minutes in a state where the temperature of the reaction mixed solution is maintained in the range of −4 to −3° C. The resin M-2a thus obtained (α-methylstyrene/4-tert-butyl-α-methylstyrene copolymer) has yield: 65 g, softening point: 153° C., number-average molecular weight (Mn): 1300, and weight-average molecular weight (Mw): 4900.

Provenance & Evidence

DOI10.6084/m9.figshare.5104873.v1
Patent numberUS08722806B2
Source datasetuspto-grants-2014_05
ORD IDord-0bfdd00a898b4e9b946cebe9547a805e
Source noteuspto-grants-2014_05