Back
HuagongsheHuagongshe Chemistry Print Report · For research reference only
HRID 1028328Generated: October 31, 2026

Ethylene → 5,6-Dihydrodicyclopentadiene Cyclopentene Ethylene

https://huagongshe.com/reaction/1028328

Reaction equation

Participants

RoleNameHCIDCharge
ReactantEthyleneHCID 6325—
ReactantCyclopenteneHCID 8882—
ReactantDihydrodicyclopentadieneHCID 95605—
ReactantTriisobutylaluminumHCID 16682931—
SolventTolueneHCID 1140—
Product5,6-Dihydrodicyclopentadiene Cyclopentene EthyleneHCID 131731425396.1%

Reaction Conditions

Temperature70 °C

Reaction Steps

5,6-dihydrodicyclopentadiene (2.7 g, 20 mmol), cyclopentene (1.4 g, 20 mmol) and magnetic bars were placed in a polymerization reactor in a nitrogen atmosphere, after which toluene was added thereto so as to obtain a total amount of 28 ml. This polymerization reactor was heated to 70° C. with stirring. A catalyst (0.69 mg, 2 μmol) represented by Formula 6, [Ph3C]+[B(C6F5)4]− (7.4 mg, 8 μmol) and triisobutylaluminum (160 mg, 800 μmol) were mixed with 2.0 ml of toluene in a dry box, after which the resulting mixture was added into the reactor using a syringe while being stirred at 70° C., and also ethylene gas was fed thereto at a pressure of 20 psig. After 6 min 30 sec, the ethylene gas was removed, and the reactor was opened, and thus the reaction was terminated. 30 ml of methanol was added and the reaction solution precipitated. Filtration was performed, thus obtaining powder. The powder was then decompressed to a vacuum at 100° C., so that the remaining solvent was removed from the precipitate, thereby obtaining 0.73 g of a polymer material. The polymer material thus obtained had a Tg of 18.4° C., a Mw of 76000 and a Mw/Mn of 1.6.

Provenance & Evidence

DOI10.6084/m9.figshare.5104873.v1
Patent numberUS08735521B2
Source datasetuspto-grants-2014_05
ORD IDord-f20371ca23f0445ba78e4d31f3112000
Source noteuspto-grants-2014_05