HuagongsheHuagongshe Chemistry Print Report · For research reference only
Cumene → Cumene
Participants
| Role | Name | HCID | Charge |
|---|---|---|---|
| Reactant | Cumene | HCID 7406 | — |
| Reactant | HCID 178418361 | HCID 178418361 | — |
| Solvent | Benzene | HCID 241 | — |
| Product | Cumene | HCID 7406 | — |
| Product | Propylene | HCID 8252 | — |
Reaction Steps
A stainless steel reaction tube with a glass-coated inside was filled with 0.1 g of a carrier molded into 0.5 to 1.0 mm in size, and a pretreatment was carried out in a stream of gaseous hydrogen of 80 ml/min in rate for three hours. 1 μl of cumene was injected into the tube at a reaction temperature of 200° C. to obtain the cracking ratios (mol %) of cumene to propylene and benzene.
Provenance & Evidence
| DOI | 10.6084/m9.figshare.5104873.v1 |
|---|---|
| Patent number | US05316996 |
| Source dataset | uspto-grants-1994_05 |
| ORD ID | ord-8d05ecedebf1457c8bdb503a7d8d58d1 |
| Source note | uspto-grants-1994_05 |