| Role | Name | HCID | Charge |
|---|
| Reactant | Propylene Glycol | HCID 1030 | — |
| Reactant | 2-Pentanone | HCID 7895 | — |
| Reactant | Isocyanate | HCID 105034 | — |
| Product | HCID 12142619 | HCID 12142619 | — |
Reaction Steps
999.28 Parts propylene glycol and 434.85 parts 2-pentanone were added to a mixing vessel equipped with a condenser, nitrogen blanket, agitator, and addition funnel. The contents were heated to about 52° C., followed by addition of 1450.97 parts MONDUR MR polymeric isocyanate while keeping the exotherm below 75° C. The addition funnel was next rinsed with 154.87 parts 2-pentanone. The reaction mixture was held at 75° C. for one to two hours until the isocyanate was consumed (thereby forming a beta-hydroxypropyl urethane polymer), then cooled to 60° C. while adding 759.92 parts propylene glycol monomethyl ether (thereby forming a beta-hydroxypropyl urethane solution). The resulting blocked polymeric isocyanate solution was mixed for 30 minutes and stored in a plastic storage vessel.
Provenance & Evidence
| DOI | 10.6084/m9.figshare.5104873.v1 |
|---|
| Patent number | US06969754B2 |
|---|
| Source dataset | uspto-grants-2005_11 |
|---|
| ORD ID | ord-da446e1fc8db49fda914c234266ee1ae |
|---|
| Source note | uspto-grants-2005_11 |
|---|