Participants
| Role | Name | HCID | Charge |
|---|
| Reactant | Toluene | HCID 1140 | — |
| Reactant | 2-(N-Methylperfluorobutanesulfonamido)ethyl methacrylate | HCID 105452 | — |
| Product | HCID 87838968 | HCID 87838968 | — |
Reaction Steps
The materials flowed through the first three zones facilitated by stirring paddles along the reaction path. Polymerization continued to substantially 100% completion by the end of zone 4, thereby forming a “living” polyisoprene reaction mixture. At the start of zone 4, the solution of diphenylethylene in cyclohexane, solids of about 12 wt %, was added by a reciprocating piston pump (at a rate of 10.0 ml/min) to the “living” polyisoprene reaction mixture. This resulted in addition of a diphenylethylene-modified polyisopropenyl chain. This chain was treated at the start of zone 5 with a purified solution of 2-(N-methylperfluorobutanesulfonamido)ethyl methacrylate in toluene, solids of 20 wt % (fed by a reciprocating piston pump at rates of 2 and 10 ml/min) to form poly(isoprene-2-(N-methylperfluorobutanesulfonamido)ethyl methacrylate) block copolymers. The overall solids content of these reactions was about 32 wt %. The total residence time for these reactions was about 25 minutes.
Provenance & Evidence
| DOI | 10.6084/m9.figshare.5104873.v1 |
|---|
| Patent number | US06903173B2 |
|---|
| Source dataset | uspto-grants-2005_06 |
|---|
| ORD ID | ord-2e95563389a84aca930f61c763017e61 |
|---|
| Source note | uspto-grants-2005_06 |
|---|