HuagongsheHuagongshe Chemistry Print Report · For research reference only
HRID 1073488Generated: October 26, 2026
Methyl Methacrylate → 2-Propenoic acid, butyl ester, polymer with 2-ethylhexyl 2-propenoate
https://huagongshe.com/reaction/1073488
Participants
| Role | Name | HCID | Charge |
|---|
| Reactant | Methyl Methacrylate | HCID 6658 | — |
| Reactant | Ethyl Methacrylate | HCID 7343 | — |
| Reactant | Butyl Methacrylate | HCID 7354 | — |
| Reactant | Styrene | HCID 7501 | — |
| Reactant | 2-Hydroxyethyl Methacrylate | HCID 13360 | — |
| Solvent | Isopropanol | HCID 3776 | — |
| Product | 2-Propenoic acid, butyl ester, polymer with 2-ethylhexyl 2-propenoate | HCID 168597 | — |
Reaction Steps
180 parts of isopropyl alcohol were put in an one-liter four-necked flask equipped with a thermometer, a stirrer, a condenser and a dropping funnel. After nitrogen replacement, the interior temperature of the flask was regulated to about 85° C. Afterwards, a monomer mixture consisting of 180 parts of methyl methacrylate, 15 parts of ethyl methacrylate, 30 parts of n-butyl methacrylate, 30 parts of styrene, 30 parts of N-n-butoxyethyl methacrylate and 15 parts of hydroxyethyl methacrylate were added dropwise into the flask with a catalyst comprising 6 parts of 2,2-azobis(2,4-dimethylvaleronitrile) over about 2 hours. After the completion of the dropwise addition, the reaction was continued at that temperature for further five hours to obtain a colorless, transparent resin solution having a solid content of about 63%.
Provenance & Evidence
| DOI | 10.6084/m9.figshare.5104873.v1 |
|---|
| Patent number | US04970126 |
|---|
| Source dataset | uspto-grants-1990_11 |
|---|
| ORD ID | ord-3703ffa6fa2940afaf881b9562c0450e |
|---|
| Source note | uspto-grants-1990_11 |
|---|