Aluminum Stearate → Ethylene brassylate

https://huagongshe.com/reaction/1074626

Reaction equation

Participants

RoleNameHCIDCharge
ReactantAluminum StearateHCID 12496—
ReactantSodium StearateHCID 2724691—
CatalystAluminum StearateHCID 12496—
CatalystLead stearateHCID 61258—
ProductEthylene brassylateHCID 6101495.9%

Reaction Steps

To demonstrate the improved yields and increased reaction rates obtained utilizing the mixed metal catalysts of this invention, batch polymerizations were identically conducted using (a) a mixed metal catalyst comprised of aluminum stearate and sodium stearate (1:1 molar ratio), (b) aluminum stearate catalyst, and (c) lead stearate catalyst. These reactions were conducted in accordance with the procedure employed in Example II utilizing 74 grams poly(ethylene brassylate) and 0.5 mole percent of the catalyst. Reactions were carried out at 310°-320° C. and 0.1-0.5 mm Hg. for four hours. The amount of distillate (crude ethylene brassylate) recovered was recorded after the first hour of reaction. With the mixed metal catalyst, 45 mls. ethylene brassylate was obtained after 1 hour and the overall yield was 95.9%. With the aluminum stearate, 36 mls. crude ethylene brassylate was obtained in the first hour and the overall yield was only 78%. Using lead stearate only 25 mls distillate was obtained after 1 hour and the yield of crude ethylene brassylate was 69.1%.

Provenance & Evidence

DOI10.6084/m9.figshare.5104873.v1
Patent numberUS04393223
Source datasetuspto-grants-1983_07
ORD IDord-3d21785902354b2ebab564dc16dbe394
Source noteuspto-grants-1983_07