Aluminum Stearate → Ethylene brassylate
Reaction equation
[C:1]([O-:17])(=[O:16])[CH2:2][CH2:3][CH2:4][CH2:5][CH2:6][CH2:7][CH2:8][CH2:9][CH2:10][CH2:11][CH2:12][C:13]([O-:15])=[O:14].[K+].[K+].[C:20]([O-])(=O)[CH2:21]CCCCCCCCCCCCCCCC.[Al+3].C([O-])(=O)CCCCCCCCCCCCCCCCC.C([O-])(=O)CCCCCCCCCCCCCCCCC>>[C:1]1(=[O:17])[O:16][CH2:21][CH2:20][O:15][C:13](=[O:14])[CH2:12][CH2:11][CH2:10][CH2:9][CH2:8][CH2:7][CH2:6][CH2:5][CH2:4][CH2:3][CH2:2]1Participants
3
Procedure
A mixed metal catalyst comprised of potassium brassylate and aluminum stearate (1:1 molar ratio of K:Al) was employed for the depolymerization of poly(ethylene brassylate) at a 1.8 wt. percent level. An 81.6 percent yield of ethylene brassylate was obtained. Comparable yields are obtained when this mixed metal catalyst is used for the depolymerization of poly(ethylene sebacate) and poly(3-oxa-pentamethylene azelate).
Sources & evidence
- ORD record
- ord-ac55d65fca16430f935b15f6ebafc0d5
- Source dataset
- uspto-grants-1983_07
- Patent number
- US04393223
Reaction notes
Loading…