HuagongsheHuagongshe Chemistry Print Report · For research reference only
Diethylene Glycol Monoethyl Ether → Ethylene brassylate
Participants
| Role | Name | HCID | Charge |
|---|---|---|---|
| Reactant | Diethylene Glycol Monoethyl Ether | HCID 8146 | — |
| Reactant | Sodium Stearate | HCID 2724691 | — |
| Reactant | Potassium Stearate | HCID 23673840 | — |
| Product | Ethylene brassylate | HCID 61014 | 73.2% |
Reaction Steps
A mixed metal catalyst prepared similarly to that of Example X, except that sodium stearate was substituted for the potassium stearate and ethyl cellusolve replaced with diethylene glycol monoethyl ether, was employed for the continuous depolymerization of poly(ethylene brassylate) in accordance with the procedure and conditions of Example I. Ethylene brassylate was continuously produced and distilled from the reactor at a rapid rate and the overall yield was 73.2%. Comparable results are obtained with a catalyst comprised of sodium benzoate and aluminum tricellusolve (Al(OCH2CH2OC2H5)3).
Provenance & Evidence
| DOI | 10.6084/m9.figshare.5104873.v1 |
|---|---|
| Patent number | US04393223 |
| Source dataset | uspto-grants-1983_07 |
| ORD ID | ord-4a23ea2bd1114aa0b97a9174535b9e69 |
| Source note | uspto-grants-1983_07 |