Styrene → Isoprene
Reaction equation
[CH2:1]=[CH:2][C:3]1[CH:8]=CC=C[CH:4]=1.C([Li])(CC)C.[CH:14]([C:16]1[CH:21]=[CH:20][CH:19]=[CH:18][C:17]=1C=C)=[CH2:15]>>[CH2:1]=[CH:2][C:3](=[CH2:4])[CH3:8].[CH2:15]=[CH:14][C:16]1[CH:21]=[CH:20][CH:19]=[CH:18][CH:17]=1Participants
5
Procedure
The polymerization was continued for 30 minutes at 70°C. Upon addition of styrene, it appeared that the reaction product of the secondary butyl lithium and divinyl benzen separated out in gel-form and did not go into solution. With the aid of the initiator gelated in this way an A-B-(A)n block copolymer was obtained by successive polymerization isoprene (50 ml) and styrene (10 ml). The properties of the resulting block copolymer are given below:
Workup
- customseparated out in gel-form
Sources & evidence
- ORD record
- ord-4f1ab892790043a5999abd58dd6dfad7
- Source dataset
- uspto-grants-1976_05
- Patent number
- US03957913
Reaction notes
Loading…