HuagongsheHuagongshe Chemie-Druckbericht · Nur für Forschungszwecke
Azobisisobutyronitrile → Vinyl acetate sodium ethylenesulfonate
Beteiligte Stoffe
| Rolle | Name | HCID | Einwaage |
|---|---|---|---|
| Edukt | Azobisisobutyronitrile | HCID 6547 | — |
| Edukt | Vinyl Acetate | HCID 7904 | — |
| Edukt | Sodium vinylsulfonate | HCID 3270262 | — |
| Lösungsmittel | Methanol | HCID 887 | — |
| Produkt | Vinyl acetate sodium ethylenesulfonate | HCID 131710246 | — |
Reaktionsschritte
A 1,000 ml. glass polymerization vessel equipped with a reflux condenser, a dropping funnel, a thermometer and a stirrer was charged with 320 parts of vinyl acetate, 130 parts of methanol, 15 parts of 30% aqueous solution of sodium ethylenesulfonate and 0.2% by mole of azobisisobutylonitrile per the vinyl acetate. After carrying out the polymerization at a temperature of 60° to 65°C. for 8 hours, the residual vinyl acetate was removed by a conventional method to give vinyl acetate-sodium ethylenesulfonate copolymer containing 2.3% by mole of sodium ethylenesulfonate unit. Then the copolymer was hydrolyzed by a conventional method to give a modified PVA of which degree of hydrolysis in vinyl acetate unit was 99% by mole.
Herkunft & Nachweise
| DOI | 10.6084/m9.figshare.5104873.v1 |
|---|---|
| Patentnummer | US03959205 |
| Quelldatensatz | uspto-grants-1976_05 |
| ORD ID | ord-3cd5ee600b35427fb7f893bffc505f65 |
| Quellennotiz | uspto-grants-1976_05 |