Styrene → Prop-2-enenitrile--ethenylbenzene (1/1)

https://huagongshe.com/reaction/1077546

Reaction equation

Participants

RoleNameHCIDCharge
ReactantStyreneHCID 7501—
ReactantAcrylonitrileHCID 7855—
Reactant1-OctanethiolHCID 8144—
ReactantCumen hydroperoxideHCID 53627471—
ProductProp-2-enenitrile--ethenylbenzene (1/1)HCID 62696—

Reaction Steps

After the liquid temperature of the latex lowered to 60° C., a mixed solution of 10 parts of acrylonitrile, 23.3 parts of styrene and 0.1 part of cumene hydroperoxide was added dropwise thereto over 2 hours to carry out polymerization. After the finish of dropping, the temperature of 60° C. was kept for 1 hour, and then a mixed solution of 10 parts of acrylonitrile, 23.3 parts of styrene, 0.03 part of n-octylmercaptan and 0.1 part of cumene hydroperoxide was again added dropwise thereto over 2 hours to carry out polymerization. After the finish of dropping, the temperature of 60° C. was kept for 2 hours, and then the reaction solution was cooled to obtain the latex of a graft compound rubber in which an acrylonitrile/styrene copolymer had been graft-polymerized onto a compound rubber comprising polydimethylsiloxane and polybutyl acrylate.

Provenance & Evidence

DOI10.6084/m9.figshare.5104873.v1
Patent numberUS05543460
Source datasetuspto-grants-1996_08
ORD IDord-0cecc74bdf134278a901129f08a54778
Source noteuspto-grants-1996_08