Back
HuagongsheHuagongshe Chemistry Print Report · For research reference only
HRID 1086691Generated: October 26, 2026

Triethylaluminum → HCID 131716738, compound

https://huagongshe.com/reaction/1086691

Reaction equation

Participants

RoleNameHCIDCharge
ReactantTriethylaluminumHCID 16682930—
ReactantMethylalumoxaneHCID 23511181—
ReactantHCID 86744437HCID 86744437—
ReactantOxaluminaneHCID 131716739—
SolventCyclohexaneHCID 8078—
ProductHCID 131716738HCID 131716738—

Reaction Steps

In this Example, a hydrogenation catalyst was prepared by first combining a methylalumoxane with nickel-2-ethylhexanoate in cyclohexane at a temperature of 25° C. and then adding triethyl aluminum. In preparing the catalyst in this Example, the amount of alumoxane combined with nickel-2-ethylhexanoate was sufficient to provide an alumoxane-nickel-2-ethylhexanoate mixture having an Al:Ni atomic ratio of 3:1. The contacting of the nickel-2-ethylhexanoate was continued for 30 minutes before the triethyl aluminum was added. When the triethyl aluminum was added, a sufficient amount was added to provide an Al (from triethyl aluminum):Ni atomic ratio of 1:1. Contacting was continued for an additional 30 minutes after the triethyl aluminum was added. For convenience, this catalyst will be referred to hereinafter as catalyst 1. This catalyst was used shortly after preparation to hydrogenate a block copolymer as summarized in Example 6.

Provenance & Evidence

DOI10.6084/m9.figshare.5104873.v1
Patent numberUS05030779
Source datasetuspto-grants-1991_07
ORD IDord-2a4d8b2955f6496992645baf7a9fd3ea