Participants
| Role | Name | HCID | Charge |
|---|
| Reactant | Sodium Stearate | HCID 2724691 | — |
| Reactant | Aluminum | HCID 5359268 | — |
| Reactant | Aluminium dihydrogen tripolyphosphate | HCID 72941519 | — |
| Solvent | Water | HCID 962 | — |
| Product | Aluminum Stearate | HCID 12496 | — |
Reaction Steps
To 300 parts of water was added 100 parts of the aluminum dihydrogen tripolyphosphate prepared above and the mixture was heated at 70±5° C. Then, 3 parts of sodium stearate and 3 parts of aluminum polychloride were added, followed by stirring at that temperature for about 1 hour. The mixture was then subjected to dehydration, drying and pulverization to give aluminum stearate-treated aluminum dihydrogen tripolyphosphate.