Participants
| Role | Name | HCID | Charge |
|---|
| Reactant | Acrylic Acid | HCID 6581 | — |
| Reactant | Butyl Acrylate | HCID 8846 | — |
| Solvent | 1,4-Dioxane | HCID 31275 | — |
| Product | HCID 22481283 | HCID 22481283 | 311.9% |
Reaction Steps
A solution was prepared of acrylic acid (10.0 g, 133 mmol) and n-butylacrylate (2.0 g, 14.41 mmol) in dioxane (200 mL). The solution was degassed by passing a rapid stream of nitrogen through it, and to the solution was added AIBN (0.6 g, 5 mol % with respect to total monomer). The solution was degassed for a further thirty minutes and the reaction was then heated to 70° C. for 17 h. The solution was cooled and precipitated into ethyl acetate (600 Ml). The ethyl acetate was decanted from the fibrous white product, the product was washed with ethyl acetate (300 Ml) followed by washing with hexane (200 Ml). The polymer was dried in vacuo to yield 9.0 g (81%) of a brittle white solid.
Provenance & Evidence
| DOI | 10.6084/m9.figshare.5104873.v1 |
|---|
| Patent number | US06060235 |
|---|
| Source dataset | uspto-grants-2000_05 |
|---|
| ORD ID | ord-f963ac2b1fdb42b88d45ae543fd0eb81 |
|---|
| Source note | uspto-grants-2000_05 |
|---|