Potassium Persulfate → Butyl Acrylate

https://huagongshe.com/reaction/1107984

Reaction equation

Participants

RoleNameHCIDCharge
ReactantPotassium PersulfateHCID 24412—
ReactantButanedioic acid, 2-sulfo-, 1,4-dioctyl ester, sodium salt (1:1)HCID 53249634—
SolventWaterHCID 962—
ProductButyl AcrylateHCID 8846—

Reaction Steps

98 parts of butyl acrylate and 2 parts of tricyclodecenyl acrylate were polymerized at 65° C. for 3 hours with stirring in 154 parts of water with addition of 2 parts of sodium dioctyl sulfosuccinate (70% strength) as emulsifier and 0.5 part of potassium persulfate. This gave an approximately 40% strength dispersion. The median particle size of the latex was about 100 nm.

Provenance & Evidence

DOI10.6084/m9.figshare.5104873.v1
Patent numberUS06063854
Source datasetuspto-grants-2000_05
ORD IDord-5b69c6c7ced447c89af690274d56f51b
Source noteuspto-grants-2000_05