Adipic Acid → Sodium silicate butadiene propylene oxide

https://huagongshe.com/reaction/1155654

Reaction equation

Participants

RoleNameHCIDCharge
ReactantAdipic AcidHCID 196—
ReactantHydrogen PeroxideHCID 784—
ReactantPropylene OxideHCID 6378—
Reactant1,3-ButadieneHCID 7845—
Reactant1-DodecanethiolHCID 8195—
ReactantSodium orthosilicateHCID 26051—
ReactantSodiumHCID 5360545—
ProductSodium silicate butadiene propylene oxideHCID 86738392—

Reaction Steps

About 50 parts by weight of an aqueous sodium silicate solution containing about 10% Na2O and 15% SiO2, 1 part by weight of adipic acid, 20 parts by weight of butadiene, 5 parts by weight of propylene oxide, 0.5 parts by weight of sodium salt of fatty acids, 0.05 to 0.1 parts by weight of ferric sulfate, 0.1 parts by weight of hydrogen peroxide, 0.01 parts by weight of benzoxyl peroxide and 0.1 parts by weight of lauryl mercaptan are mixed in a closed system at ambient to 50° C. while agitating at about 0.40 to 6 psiq for 30 to 120 minutes; then the mixture is heated to 70° to 100° C. at ambient pressure for 10 to 30 minutes. The reaction is complete within 24 hours thereby producing an emulsion of poly(sodium silicate-butadiene-propylene oxide) copolymer.