HuagongsheHuagongshe Chemistry Print Report · For research reference only
2-ethylhexanoic acid tin(II) salt → Ethyl carbamate;bis(2-methylprop-2-enoic acid)
Participants
| Role | Name | HCID | Charge |
|---|---|---|---|
| Reactant | 2-ethylhexanoic acid tin(II) salt | HCID 9318 | — |
| Reactant | Trimethylhexa-1,6-diyl diisocyanate | HCID 3033881 | — |
| Product | Ethyl carbamate;bis(2-methylprop-2-enoic acid) | HCID 21885196 | — |
Reaction Steps
To a mechanically-stirred mixture of 28.59 weight parts of trimethylhexamethylene diisocyanate and 0.04 weight part of stannous octoate in a reactor and purged with dry air, there is added 44.80 weight parts of polytetramethylene ether glycol, while maintaining the reaction temperature at 50° to 60° C. After the addition is complete, the mixture is heated to 70° to 80° C. and held for 3 hours. A 26.58 weight parts of hydroxyethyl methacrylate (HEMA) was added and the mixture was stirred at 70° to 80° C. until the percent NCO assay was below 0.01%.
Provenance & Evidence
| DOI | 10.6084/m9.figshare.5104873.v1 |
|---|---|
| Patent number | US04814423 |
| Source dataset | uspto-grants-1989_03 |
| ORD ID | ord-da0fdd3ad703426f857a99254d42abae |
| Source note | uspto-grants-1989_03 |