HuagongsheHuagongshe Chemistry Print Report · For research reference only
Styrene → HCID 178454688, compound
Participants
| Role | Name | HCID | Charge |
|---|---|---|---|
| Reactant | Styrene | HCID 7501 | — |
| Reactant | HCID 178454790 | HCID 178454790 | — |
| Catalyst | Azobisisobutyronitrile | HCID 6547 | — |
| Solvent | Dichloromethane | HCID 6344 | — |
| Product | HCID 178454688 | HCID 178454688 | 209.9% |
Reaction Steps
A 6-ml flask was charged with 0.489 g of pyrithione methacrylate (2.5 mmole), 2.6 ml of styrene (22.5 mmole) and 0.083 g of AIBN (0.5 mmole). The flask was sealed and placed in an oven at 80° C. for 16 hours. After cooling to room temperature, the product was diluted with 10 ml of methylene chloride and filtered. The solution was concentrated via roto-evaporation and 1.66 g of the desired product was isolated as a yellow polymeric material for a 56.9% yield. The structure was confirmed by NMR and IR. Similar results were obtained by employing either acetyl peroxide, benzoyl peroxide, or lauryl peroxide as the radical initiator.
Provenance & Evidence
| DOI | 10.6084/m9.figshare.5104873.v1 |
|---|---|
| Patent number | US04632881 |
| Source dataset | uspto-grants-1986_12 |
| ORD ID | ord-88e75d72b68f42df864835972a32fd39 |
| Source note | uspto-grants-1986_12 |