HuagongsheHuagongshe Chemistry Print Report · For research reference only
HRID 1256931Generated: November 3, 2026
Styrene → Benzene, ethenyl-, polymer with 1,3-butadiene
https://huagongshe.com/reaction/1256931
Participants
| Role | Name | HCID | Charge |
|---|
| Reactant | Styrene | HCID 7501 | — |
| Reactant | 1,3-Butadiene | HCID 7845 | — |
| Reactant | Butyllithium | HCID 178418339 | — |
| Solvent | Cyclohexane | HCID 8078 | — |
| Product | Benzene, ethenyl-, polymer with 1,3-butadiene | HCID 62697 | — |
Reaction Steps
A polymer solution of polystyrene-polybutadiene block copolymer 2b was prepared as follows. 1885 grams of cyclohexane (with 120ppm THF) solvent was added into a 5-liter autoclave and heated to 58° C. 89.0 grams of styrene monomers and 4.2 grams of 15 wt.% n-butyl lithium were added sequentially to start polymerization. While the styrene monomers were almost completely reacted, 218grams of butadiene monomers were added to continue polymerization until the butadiene monomers were almost completely reacted. The reaction was terminated by adding 1.27 grams of water. 0.7 phr of antioxidant (mixture of phosphite series Irgafos 126 and phenolic series Irganox 1076 antioxidants) was added following by well stirring, and thus the polymer solution of the polystyrene - polybutadiene block copolymer 2b was obtained.
Provenance & Evidence
| DOI | 10.6084/m9.figshare.5104873.v1 |
|---|
| Patent number | US08461246B2 |
|---|
| Source dataset | uspto-grants-2013_06 |
|---|
| ORD ID | ord-ac280491bc5e4e42ba528983b0232d45 |
|---|
| Source note | uspto-grants-2013_06 |
|---|