Back
HuagongsheHuagongshe Chemistry Print Report · For research reference only
HRID 1260139Generated: October 29, 2026

Stearic Acid → Zinc Stearate

https://huagongshe.com/reaction/1260139

Reaction equation

Participants

RoleNameHCIDCharge
ReactantStearic AcidHCID 5281—
ReactantZincHCID 23994—
ProductZinc StearateHCID 11178—

Reaction Conditions

Temperature150 °C

Reaction Steps

Stearic acid (75 grams) was added to 500 gram of zinc clay RA. The mixture was attrition milled for two hours and then heated at 150° C. for one more hour. The product again was attrition milled and then jet milled through a CJ-10 jet mill manufactured by Nisshin Engineering Co. Ltd. of Japan. The final product was sieved through a 200 mesh sieve to produce zinc stearate clay RB. There is some loss of material through dusting at the various milling processes. Its properties are listed below:

Provenance & Evidence

DOI10.6084/m9.figshare.5104873.v1
Patent numberUS08470727B2
Source datasetuspto-grants-2013_06
ORD IDord-ca9ce2070d7a49829aa17232f7b797ab
Source noteuspto-grants-2013_06