Back
HuagongsheHuagongshe Chemistry Print Report · For research reference only
HRID 1260140Generated: October 25, 2026

Ammonia → Zinc Stearate

https://huagongshe.com/reaction/1260140

Reaction equation

Participants

RoleNameHCIDCharge
ReactantAmmoniaHCID 222—
ReactantCarbon DioxideHCID 280—
ReactantStearic AcidHCID 5281—
ReactantZincHCID 23994—
ReactantCarbon dioxide, ammoniateHCID 18185886—
ProductZinc StearateHCID 11178—
ProductAmmonium StearateHCID 9861187—

Reaction Conditions

Temperature60 °C

Reaction Steps

An ammonium stearate solution was prepared by mixing 113.5 grams of stearic acid with 567 grams of ammonia/carbon dioxide solution containing 12% of ammonia and 10% of carbon dioxide. The solution was sprayed onto 756 grams of zinc clay R591, then the mixture was mixed well and heated to 60° C. The resulting powder was heated at 110° C. for 18 hours. The dried powder was attrition milled again and then sieved with a 140 mesh sieve. The product was jet milled with the Nissen jet mill (see Example 2) to produce zinc stearate clay RC. There is some loss of material through dusting at the various milling processes. Its properties are listed below:

Provenance & Evidence

DOI10.6084/m9.figshare.5104873.v1
Patent numberUS08470727B2
Source datasetuspto-grants-2013_06
ORD IDord-3ffdb6c3bcef473585eca8bc946b6608
Source noteuspto-grants-2013_06