A powder of commercial magnesium oxide (80 g) calcined at 550° C. and 282 g of phenol were charged in a ball mill and mixed at 150° C. for 16 hours. Phenol was thoroughly removed by vacuum evaporation to give magnesium phenolate-containing magnesium oxide of particle sizes 10-16 mesh.

WORKUP

后处理

  1. customcalcined at 550° C.
  2. additionmixed at 150° C. for 16 hours
  3. customPhenol was thoroughly removed by vacuum evaporation