Water → Styrene
Reaction equation
[CH2:1]=[CH:2][C:3]1[CH:8]=[CH:7][CH:6]=[CH:5][CH:4]=1.[C:9]([OH:14])(=[O:13])[C:10](C)=[CH2:11].[CH3:15][O:16][CH2:17]CO.[OH2:20]>>[CH2:1]=[CH:2][C:3]1[CH:8]=[CH:7][CH:6]=[CH:5][CH:4]=1.[C:17]([O:16][CH3:15])(=[O:20])/[CH:11]=[CH:10]\[C:9]([O-:14])=[O:13]Participants
6
Procedure
In the case of a solution polymerization, for example, 23 parts of styrene, 24 parts of methacrylic butyl, 23 parts of methacrylic acid, and 10 parts of a polyethylene glycol monomethyl ester of methacrylic acid are fed in water-soluble solvent (e.g., butyl cellosolve) at 80 to 140° C. under an ambient nitrogen atmosphere, and are pre-mixed. The mixture is then copolymerized for 4 to 5 hours with dripping a polymerization initiator, then 20 parts of the AD copolymer (e.g., obtained from 10 parts of styrene and 10 parts of monomethyl maleate) is added to the mixture, and is heated and stirred for 2 to 8 hours.
Workup
- customIn the case of a solution polymerization
- additionare pre-mixed
- customcopolymerized for 4 to 5 hours
Sources & evidence
- ORD record
- ord-6159cbb21363498d89b5a4fbccf6a164
- Source dataset
- uspto-grants-2003_04
- Patent number
- US06548460B1
Reaction notes
Loading…