An AB block polymer of styrene-isoprene was prepared by adding 0.42 ml. of 1.18 N sec-butyl lithium to a mixture of 10 g. of styrene of 175 ml. of benzene and 5 ml. of tetrahydrofuran at room temperature. The mixture was allowed to polymerize for 2 hours and 40 g. of dry air-free isoprene was added and the polymerization continued for 2 additional hours. The product was isolated by precipitation into methanol, yielding 27.5 g. of block polymer dispersant.
Provenance & Evidence
| DOI | 10.6084/m9.figshare.5104873.v1 |
|---|---|
| Patent number | US03972963 |
| Source dataset | uspto-grants-1976_08 |
| ORD ID | ord-bee14c231fba49618fde7a2c45ed7e09 |
| Source note | uspto-grants-1976_08 |