Participants
| Role | Name | HCID | Charge |
|---|
| Reactant | Styrene | HCID 7501 | — |
| Reactant | Maleic Anhydride | HCID 7923 | — |
| Solvent | O-Xylene | HCID 7237 | — |
| Product | HCID 19842620 | HCID 19842620 | — |
Reaction Steps
A separable flask equipped with a stirrer and a cooler was charged with 30 g of a maleic anhydride modified hydrogenated styrene-isoprene-styrene block copolymer (styrene content: 35%, degree of hydrogenation: 96%, maleic anhydride content: 0.03 meq/g) and 100 g of xylene. Separately, a solution of 3-aminophenylboronic acid ethylene glycol ester in xylene was prepared by dehydrating distillation of a mixture of 20 g of xylene, 310 mg of 3-aminophenylboronic acid hydrate and 120 mg of ethylene glycol, and the solution was fed to the flask. The reaction mixture was heated at 140° C. for 3 hours. After cooling o E the reaction mixture, the polymer that formed was reprecipitated from methanol containing 0.1% of ethylene glycol, and dried, to give a hydrogenated styrene-isoprene-styrene copolymer having an MI of 2 g/10 min and 0.028 meq/g of boronic acid ethylene glycol ester groups on side chains.
Provenance & Evidence
| DOI | 10.6084/m9.figshare.5104873.v1 |
|---|
| Patent number | US05466748 |
|---|
| Source dataset | uspto-grants-1995_11 |
|---|
| ORD ID | ord-984be7e81de74c9598c8d4cde841c9c4 |
|---|
| Source note | uspto-grants-1995_11 |
|---|