Styrene → Styrene octene

https://huagongshe.com/reaction/1369062

Reaction equation

Participants

RoleNameHCIDCharge
ReactantStyreneHCID 7501—
Reactant1-OcteneHCID 8125—
ReactantBis(isobutyl)aluminum chlorideHCID 15688—
ProductStyrene octeneHCID 86748443—

Reaction Steps

A styrene-octene copolymer was prepared in an inert environment under standard temperature and pressure by mixing 47.1 grams of styrene with 453.0 grams of octene in a beaker. After stirring, 4.0 milliliters of a 25% DIBAC solution was added to the beaker. The mixture was held for 30 minutes without stirring. A 3.0 milliliter portion of the catalyst mixture prepared in Example 1 was added to the beaker while stirring continuously. The entire mixture was allowed to react. The subsequent copolymer was subsequently tested and found to have a 95.3% conversion to polymer with an inherent viscosity of 28.1 deciliters/gram.

Provenance & Evidence

DOI10.6084/m9.figshare.5104873.v1
Patent numberUS06576732B1
Source datasetuspto-grants-2003_06
ORD IDord-60af3b73b9874afda3fe3e28d1304e6e