Participants
| Role | Name | HCID | Charge |
|---|
| Reactant | Water | HCID 962 | — |
| Reactant | Styrene | HCID 7501 | — |
| Reactant | Sodium Lauryl Sulfate | HCID 3423265 | — |
| Reactant | Benzene, 1-(chloromethyl)-3(or 4)-ethenyl- | HCID 11768772 | — |
| Solvent | Sodium Chloride | HCID 5234 | — |
| Product | HCID 22420136 | HCID 22420136 | — |
Reaction Steps
Four hundred cc. distilled water was boiled in a 1 liter three-neck flask under nitrogen gas and then cooled to room temperature. Six g. of sodium lauryl sulfate was added and stirred to form a solution. The solution was further cooled to 15° C., and a mixture of 39 g. vinylbenzyl chloride and 61 g. styrene was added with vigorous agitation, followed by 1 g. of K2S2O8 and 1 g. of Na2S2O5. The mixture was heated slowly to 35° C. and held at this temperature overnight. The resultant copolymer latex was coagulated in 10% NaCl solution, filtered, and washed with distilled water and then with methanol. The wet copolymer was then dried at room temperature in a forced-convection oven. A solution of the vinylbenzyl chloride-styrene copolymer in DMF was then prepared for membrane casting.
Provenance & Evidence
| DOI | 10.6084/m9.figshare.5104873.v1 |
|---|
| Patent number | US04584246 |
|---|
| Source dataset | uspto-grants-1986_04 |
|---|
| ORD ID | ord-f585081129eb4cda80bb1d323fafccb0 |
|---|
| Source note | uspto-grants-1986_04 |
|---|