HuagongsheHuagongshe Chemistry Print Report · For research reference only
HRID 1383864Generated: October 31, 2026
Allyl glycidyl ether → Glycidyloxypropyltrimethylsilane
https://huagongshe.com/reaction/1383864
Participants
| Role | Name | HCID | Charge |
|---|
| Reactant | Allyl glycidyl ether | HCID 7838 | — |
| Reactant | Trimethylsilane | HCID 70435 | — |
| Catalyst | Platinum | HCID 23939 | — |
| Product | Glycidyloxypropyltrimethylsilane | HCID 11816314 | — |
Reaction Steps
Allyl glycidyl ether (30.3 g, 0.266 moles) and 3 mg of platinum catalyst are weighed into a 300 mL laboratory autoclave. The autoclave, together with its contents, is cooled in an acetone/dry ice bath in an atmosphere of argon and 19.7 g of trimethylsilane (0.266 moles with a boiling point of 6.7° C.) are siphoned over from the condensed phase. The autoclave is closed and heated to 130° C. At the same time, the internal pressure increases to 7.6 bar and then drops again to 3.2 bar, indicating a reaction.
Provenance & Evidence
| DOI | 10.6084/m9.figshare.5104873.v1 |
|---|
| Patent number | US06255511B1 |
|---|
| Source dataset | uspto-grants-2001_07 |
|---|
| ORD ID | ord-5cf358facc6f434d83a90811e4fe650f |
|---|
| Source note | uspto-grants-2001_07 |
|---|