Participants
| Role | Name | HCID | Charge |
|---|
| Reactant | Acetone | HCID 180 | — |
| Reactant | 4-Vinylphenol | HCID 62453 | — |
| Catalyst | Iodine | HCID 807 | — |
| Solvent | Acetonitrile | HCID 6342 | — |
| Product | 4-Ethynylphenol | HCID 32758 | 16.6% |
Reaction Steps
51.0 g of the same p-vinylphenol fraction as used in Example 1, obtained by vacuum flash distillation was placed in a 300-ml flask together with 51.0 g of acetone. To the resulting mixture being stirred and cooled to 0° C. was dropwise added 1.0 ml of an acetonitrile solution containing 0.02 g of iodine. A polymerization reaction was conducted for 1 hour at 0° C. to obtain 8.3 g of a poly(p-vinylphenol). The polymer had a Mw of 13,800, a Mn of 11,200, a light transmittance at 248 nm, of 76.3% and a light transmittance at 450 nm, of 95.0%.
Provenance & Evidence
| DOI | 10.6084/m9.figshare.5104873.v1 |
|---|
| Patent number | US06258901B1 |
|---|
| Source dataset | uspto-grants-2001_07 |
|---|
| ORD ID | ord-634fd7131bd34855b5551491f9314b05 |
|---|
| Source note | uspto-grants-2001_07 |
|---|