Reaction Steps
The following were mixed with 1,6-HG (39.3 parts) to prepare homogeneous glycol components: a polyester diol (243.5 parts) having an Mn of 1000 yielded from 1, 4-BD, and adipic acid; a polyester diol (243.5 parts) having an Mn of 2600 yielded from 1,4-BD, ethylene glycol, and adipic acid; and a polyester diol (324.7 parts) having an Mn of 1500 yielded from 1,6-HG and isophthalic acid. The glycol components were mixed with HDI, and the mixture was supplied at a flow rate ratio of 100:17.5 from a hopper of a biaxial extruder, the temperature of which was adjusted to about 190° C. The mixture was kneaded, and simultaneously resinified to yield a polyurethane resin.
Provenance & Evidence
| DOI | 10.6084/m9.figshare.5104873.v1 |
|---|---|
| Patent number | US08912281B2 |
| Source dataset | uspto-grants-2014_12 |
| ORD ID | ord-fee9698307914028bff47108c2de8c1a |
| Source note | uspto-grants-2014_12 |