Back
HuagongsheHuagongshe Chemistry Print Report · For research reference only
HRID 1416808Generated: November 3, 2026

Azobisisobutyronitrile → Styrene

https://huagongshe.com/reaction/1416808

Reaction equation

Participants

RoleNameHCIDCharge
ReactantAzobisisobutyronitrileHCID 6547—
ReactantStyreneHCID 7501—
Reactant1-(Tert-butoxy)-4-ethenylbenzeneHCID 577531—
Solvent1,4-DioxaneHCID 31275—
ProductStyreneHCID 7501—
Product4-VinylphenolHCID 62453—

Reaction Steps

300 g of p-t-butoxystyrene, 30 g of styrene, and 1.6 g of azobis-iso-butylonitrile were dissolved in 330 g of dioxane, and reacted for 12 hours under a nitrogen atmosphere at 70° C. After the reaction, unreacted monomers were removed to obtain a copolymer of p-hydroxystyrene and styrene. This resin was hydrolyzed with an acid to produce 180 g of a copolymer of p-hydroxystyrene and styrene with Mw of 18,000. NMR measurement confirmed that the molar ratio of p-hydroxystyrene and styrene was 85:15.

Provenance & Evidence

DOI10.6084/m9.figshare.5104873.v1
Patent numberUS05916729
Source datasetuspto-grants-1999_06
ORD IDord-9753550d3dfe4796a9a9912c63a210a0
Source noteuspto-grants-1999_06